MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Avient Versalloy™ HC 9210-55N Thermoplastic Elastomer (TPE)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Versalloy™ HC 9210-55N is a TPV alloy targeted for injection molding healthcare applications such as disposable medical items, syringe stoppers, and soft-touch overmolding onto surgical grips. Product exhibits exceptional flow properties and surface aesthetics. * Excellent Flow for Long, Thin Flow Paths * Exceptional Colorability * Overmold Adhesion to Polypropylene * Superior Surface Aesthetics * USP Class VI (please see Notes)

Versalloy™ HC 9210-55N can be recycled as a filler or impact modifier for polyolefins, or can be recycled by grinding and reintroduction to the molding process. Similar to PP or PE recycling process, if separated appropriately, it can be recycled many times. Municipality waste stream recycle code is 7 which is designated for Other. Please contact GLS Thermoplastic Elastomers for a copy of our Recyclability Compliance letter.

Color concentrates with polypropylene (PP) carrier are most suitable for coloring Versalloy™ HC 9210-55N. Improved color dispersion can be achieved by using higher melt flow concentrates (with a melt flow from 25 - 40 g/10 min). Typical loadings for color concentrates are 1% to 5% by weight. Concentrates based on PVC should not be used. A high color match consistency can be obtained by the use of precolored compounds available from GLS. The final determination of color concentrate suitability should be determined by customer trials. Purge thoroughly before and after use of this product with a low flow (0.5 - 2.5 MFR) polyethylene (PE) or polypropylene (PP). Regrind levels up to 20% can be used with Versalloy™ HC 9210-55N with minimal property loss, provided that the regrind is free of contamination. To minimize losses during molding, the melt temperature should remain as low as possible. The final determination of regrind effectiveness should be determined by the customer. Versalloy™ HC 9210-55N has good melt stability. Maximum residence times may vary, depending on the size of the barrel. Generally, the barrel should be emptied if it is idle for periods of 8 - 10 minutes or longer. Drying is not Required Injection Speed: 1 to 5 in/sec 1st Stage - Boost Pressure: 300 to 700 psi 2nd Stage - Hold Pressure: 70% of Boost Hold Time (Thick Part): 4 to 10 sec Hold Time (Thin Part): 1 to 3 sec

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.888 g/ccASTM D792
Viscosity 6200 cP
@Shear Rate 11200 1/s,
Temperature 200 °C
ASTM D3835
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 5310 sec; ASTM D2240
Tensile Strength at Break 4.00 MPa
@Temperature 23.0 °C
Die C2 hr; ASTM D412
Tensile Stress at Strain 1.44 MPa
@Strain 100 %,
Temperature 21.0 °C
Die C2 hr; ASTM D412
 2.31 MPa
@Strain 300 %,
Temperature 23.0 °C
Die C2 hr; ASTM D412
Elongation at Break 610 %
@Temperature 23.0 °C
Die C2 hr; ASTM D412
Tear Strength 21.0 kN/m
@Temperature 21.0 °C
Die C2 hr; ASTM D624
Compression Set 20 %
@Temperature 23.0 °C,
Time 79200 sec
ASTM D395B
 38 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM D395B
 44 %
@Temperature 100 °C,
Time 79200 sec
ASTM D395B
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 149 - 188 °C
Middle Barrel Temperature 160 - 199 °C
Front Barrel Temperature 171 - 210 °C
Nozzle Temperature 171 - 210 °C
Mold Temperature 15.6 - 26.7 °C
Back Pressure 0.689 - 1.38 MPa
Screw Speed 50 - 100 rpm
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes
 Yes
 
Descriptive Properties
AppearanceNatural Color
FeaturesGood Colorability
 Good Processability
 Good Surface Finish
 Halogen Free
 High Flow
 Non-Phthalate Plasticizer
 Recyclable Material
FormsPellets
Generic MaterialTPE
Generic NameThermoplastic Elastomer (TPE)
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
RoHS ComplianceRoHS Compliant
Suggested Max Regrind20%
UsesFlexible Grips
 Medical/Healthcare Applications
 Overmolding
 Soft Touch Applications
 Thin-walled Parts

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Advanced Elastomer Systems Santoprene® 181-55 Thermoplastic Rubber
Advanced Elastomer Systems Santoprene® 281-64 Thermoplastic Rubber
Advanced Elastomer Systems Santoprene® 283-40 Thermoplastic Rubber
Avient Dynaflex™ G2706-1000-00 Thermoplastic Elastomer (TPE)
Avient Versaflex™ HC MT555 Thermoplastic Elastomer (TPE)

PH0POL1260 / 145829

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.