MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexWeb® A1-139-3 High strength aramid honeycomb
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoset; Aramid; Phenolic

Material Notes: Description: Non-metallic honeycombs are manufactured from high temperature resistant aramid paper formed into a honeycomb structure, and coated with a phenolic resin. The combination of aramid paper and phenolic resin gives types A1 and A10 their superior strength, toughness and chemical resistance. The honeycomb cell shape is normally hexagonal for optimum mechanical properties. It can also be over expanded to produce a rectangular cell shape and provide improved drapeability for the production of curved parts.

Key Features:

  • High mechanical strength at low densities.
  • Outstanding resistance to corrosive attack by chemicals.
  • Excellent resistance to impact damage and moisture.
  • Fire retardant and self extinguishing.
  • Low smoke and toxic gas emission.
  • Highly resistant to fungal growth.
  • Good dielectric properties, transparent to radio and radar waves.
  • Easily cut and machined to shape and can be heat formed.
  • Low thermal conductivity.
  • Compatible with most lightweight reinforced composite materials, providing a good bonding surface for Redux® adhesives and self adhesive prepreg systems.
  • Easy single curvature forming of over-expanded honeycomb.
Applications: Aerospace: Helicopter blades, fairings, interior panels, flooring, control surfaces, flaps, engine nacelles; HexWeb A1 honeycomb is qualified to all major aerospace specifications; Industrial: Marine and ground transportation, interior panels, flooring, bulkheads, hatches; Racing boat shells; High performance car chassis and body panels; Precision optical equipment; Desiccant and filtration systems; Radar reflectors, covers and emitters.
HexWeb A10 honeycomb is recommended for all industrial applications.

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.139 g/cc0.00502 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 14.0 MPa2030 psi
Compressive Modulus 0.580 GPa84.1 ksi
Shear Modulus 67.0 GPa9720 ksiW Direction
 113 GPa16400 ksiL Direction
Shear Strength 1.88 MPa273 psiW Direction
 3.40 MPa493 psiL Direction

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHEXCB9238 / 322394

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.