MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Bhansali Engineering Santron IMS1000 Sparkle SAN Resin
Categories: Polymer; Thermoplastic; SAN Polymer; Styrene Acrylonitrile (SAN), Transparent

Material Notes: High Transparent SAN

Information provided by Bhansali

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.07 g/cc1.07 g/ccASTM D792
Linear Mold Shrinkage 0.0040 - 0.0050 cm/cm0.0040 - 0.0050 in/inASTM D955
Melt Flow 35 g/10 min
@Load 10.0 kg,
Temperature 220 °C
35 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 122122ASTM D785
Tensile Strength, Yield  63.7 MPa
@Thickness 3.20 mm
9250 psi
@Thickness 0.126 in
Type I, 5 mm/min; ASTM D638
 68.6 MPa
@Thickness 3.20 mm
9960 psi
@Thickness 0.126 in
Type I, 50 mm/min; ASTM D638
Flexural Yield Strength 98.1 MPa
@Thickness 6.40 mm
14200 psi
@Thickness 0.252 in
5 mm/min; ASTM D790
Izod Impact, Notched 0.294 J/cm
@Thickness 3.20 mm
0.551 ft-lb/in
@Thickness 0.126 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C
@Thickness 6.40 mm
203 °F
@Thickness 0.252 in
Method A; ASTM D648
Flammability, UL94 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %transparent; thickness not quantified

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
INEOS Styrolution Absolan® 2500 SAN
INEOS Styrolution Absolan® 2150 SAN
INEOS Styrolution Absolan® 2300 Sparkle SAN
INEOS Styrolution Absolan® 2300 SAN
Bhansali Engineering Santron IMS1000M SAN Resin

PBHANS939 / 178107

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.