MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nouryon Perkadox 16-40XPS Di(4-tert-butylcyclohexyl) peroxydicarbonate
Categories: Other Engineering Material

Material Notes: Peroxydicarbonate used for curing unsaturated polyester resins and methacrylic resins. The material is formulated to a pumpable suspension which allows continuous operation and safe handling.

CAS number: 15520-11-3

EINECS/ELINCS No.: 239-557-1

Applications: Perkadox 16-40XPS is a smooth peroxydicarbonate paste which is used for the curing of unsaturated polyester resins and methacrylic resins mainly in the temperature range of 60°C (140°F) and higher. The Perkadox 16-40XPS paste dissolves readily in a resin formulation without the need for additional solvents. There is no need for extra handling or long mixing times.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³
Half-life  0.100
@Temperature 82.0 °C
0.100
@Temperature 180 °F
[hr]
 1.00
@Temperature 64.0 °C
1.00
@Temperature 147 °F
[hr]
 10.0
@Temperature 48.0 °C
10.0
@Temperature 118 °F
[hr]
Viscosity 2000 - 10000 cP2000 - 10000 cP
Molecular Weight 398.5 g/mol398.5 g/mol
Storage Temperature <= 15.0 °C<= 59.0 °F
 
Thermal PropertiesMetricEnglishComments
Decomposition Temperature 45.0 °C113 °FSelf-Accelerating Decomposition Temperature
 
Processing PropertiesMetricEnglishComments
Shelf Life 3.00 Month3.00 Month
 
Descriptive Properties
AppearanceWhite paste
Assay37.5-40.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY753 / 286276

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.