MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Precision Polymer Engineering Q70R Polyurethane Rubber
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced; Rubber or Thermoset Elastomer (TSE)

Material Notes: Peroxide cured, red Polyurethane Rubber, 65-75 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG714, B14, EO14, EO34. ASTM & ISO designation = AU.

Applications: Excellent abrasion resistance and tensile strength, with fluid compatibility approaching that of NBR. Polyurethane seals provide outstanding performance in hydraulic systems, which are prone to abrasive contamination and high shock loads. Good resistance to weathering and ozone but poor against water and high temperature.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7070°IRHD; ASTM D1415
 8585°IRHD, +15 change after 70 hours @ 100°C; ASTM D1415
Tensile Strength, Yield 11.2 MPa1620 psi-20% change after 70 hours @ 100°C; ASTM D412
 14.0 MPa2030 psiASTM D412
Elongation at Break 150 %150 %-40% change after 70 hours @ 100°C; ASTM D412
 250 %250 %ASTM D412
Compression Set 25 %
@Temperature 100 °C,
Time 252000 sec
25 %
@Temperature 212 °F,
Time 70.0 hour
ASTM D395
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 100 °C212 °F
Minimum Service Temperature, Air -35.0 °C-31.0 °FNon-brittle after 3 minutes
 -30.0 °C-22.0 °F
Flash Point >= 204 °C>= 399 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPRECI218 / 57942

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.