MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Ganpati Exim N299 Carbon Black
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Improved fine carbon black with increased structure. Provides optimum wear resistance, high modulus at 300% and low hysteresis, combining with good processing properties. Tire tread, retread compounds. Industrial rubber goods.

Information provided by Ganpati Exim PVT. LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.335 g/ccPour
Specific Surface Area 97 m²/gExternal, Based on the Statistical Thickness Surface Area Method, (D6556)
 
Mechanical PropertiesOriginal ValueComments
300% Modulus 0.700 MPaIRB 6
 
Descriptive Properties
DBP Absorption Number124 cm3/100g
DBP Absorption Number of Compressed Sample104 cm3/100g
Iodine Number108 g/kg
Nitrogen Adsorption Number104 m2/g
Tint Index1.13ITRB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGANPATI002 / 317286

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.