Hostacom X 4305 HL86 304986 is a 22% talc filled PP copolymer, with good stiffness, good toughness and superior UV resistance suitable for exterior applications. Product is available as a customized color matched, pellet form. This grade is delivered in 304986 color version. Applications: Exterior TrimInformation provided by LyondellBasell. |