MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Kingfa FRHIPS-980 Flame Retardant Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Flame Retardant

Material Notes:
    Features:
  • UL 94 V-0 @ 1.6mm, V-0 @ 3.2mm
  • Excellent balance properties, Non-DPO
  • Excellent heat stability & electrical property
  • Color tailor-made for client

    Applications:
  • Injection molding
  • Gas assistant molding
  • TV, printer, photocopier and fax housing
  • Electric and electronic cabinet

Information Provided by Kingfa Sci. & Tech. Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 g/cc
@Temperature 23.0 °C
1.15 g/cc
@Temperature 73.4 °F
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
@Temperature 23.0 °C
0.0040 - 0.0060 in/in
@Temperature 73.4 °F
ASTM D955
Melt Flow 10 g/10 min
@Load 5.00 kg,
Temperature 200 °C
10 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 24.0 MPa3480 psi50mm/min; ASTM D638
Elongation at Break 40 %40 %50mm/min; ASTM D638
Flexural Strength 39.0 MPa5660 psi2mm/min; ASTM D790
Flexural Modulus 2.20 GPa319 ksi2mm/min; ASTM D790
Izod Impact, Notched 1.25 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
2.34 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
 
Thermal PropertiesMetricEnglishComments
Hot Ball Pressure Test 85.0 °C
@Thickness 2.00 mm
185 °F
@Thickness 0.0787 in
IEC695-10-2
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
@Thickness 6.40 mm
167 °F
@Thickness 0.252 in
ASTM D648
Flammability, UL94  V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
 V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature <= 250 °C<= 482 °F
Rear Barrel Temperature 182 - 205 °C360 - 401 °FStart Point: 190°C
Middle Barrel Temperature 205 - 230 °C401 - 446 °FStart Point: 215°C
Front Barrel Temperature 215 - 240 °C419 - 464 °FStart Point: 225°C
Melt Temperature 220 - 245 °C428 - 473 °FStart Point: 230°C
Mold Temperature 30.0 - 60.0 °C86.0 - 140 °FStart Point: 50°C
Drying Temperature 70.0 °C
@Time 7200 sec
158 °F
@Time 2.00 hour
Pre-dry
Back Pressure 5.00 - 15.0 MPa725 - 2180 psi
 
Descriptive Properties
Injection SpeedSlow to Moderate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 1008 Steel, cold drawn bar, 19-32 mm (0.75-1.25 in) round
AISI 1006 Steel, CQ, DQ, and DQSK sheet, 1.6-5.8 (0.06-0.23 in) mm thick
Stellarchem GP-980 TPE Compound
Shuman 980-05V0 Grey Polycarbonate Glass Filled
Michelman® Plate Kote™ 980 KOSHER Water based OPV

PKINGF100 / 104359

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.