MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Esstech X-739-0000 Ethoxylated Bis Phenol A Dimethacrylate, C39H56O12
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: This form of EBPADMA has 8 units of ethoxylation. Increasing the ethoxylated chain length increases the mobility of the molecule and therefore it reactivity and degree of conversion. Listed on the Toxic Substance Control Act List. CAS # 41637-38-1.

Information provided by ESSTECH, Inc.

Key Words: C39H56O12
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.122 g/cc1.122 g/cc
Viscosity 525 cP
@Temperature 25.0 °C
525 cP
@Temperature 77.0 °F
Molecular Weight 716.8 g/mol716.8 g/mol
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5181.518
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.20 %<= 0.20 %
 
Descriptive Properties
Acidity (% Methacrylic Acid)< 0.05
MeHQ Inhibitor (ppm)150-250
Purity (%)> 87

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PESST036 / 108307

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.