MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Fainplast Compounds Hax™ HFX 519 Crosslinkable HFFR Cable Compound  (discontinued **)
Categories: Polymer; Thermoplastic; Polyolefin; Polyolefin, Wire/Cable Grade

Material Notes: Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalyst

Grade description:
• Sheathing, Insulation

Information provided by Fainplast Compounds

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.34 - 1.38 g/ccISO 1183
Melt Flow 3.0 g/10 min
@Load 21.6 kg,
Temperature 150 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 35 - 41ISO 868
Tensile Strength 12.0 MPaCrosslinked specimen; ISO 527
Elongation at Break 270 %Crosslinked specimen; ISO 527
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+16 ohm-cmASTM D257
 
Thermal PropertiesOriginal ValueComments
Oxygen Index 30 %ISO 4589
 
Processing PropertiesOriginal ValueComments
Processing Temperature 120 - 200 °C
Shelf Life 3.00 Month
@Temperature 30.0 °C
Moisture absorption after extended storage

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Fainplast Compounds Hax™ HFX 500S Crosslinkable HFFR Cable Compound
Borealis Casico™ FR4820 Natural Low Smoke Zero Halogen Flame Retardant Insulation Compound for Building Energy Cables
Phillips 66 Synterra™ 32 Wire Rope Lubricant 32
Fainplast Compounds Hax™ HFX 521 Crosslinkable HFFR Cable Compound
Fainplast Compounds Hax™ HFX 500 Crosslinkable HFFR Cable Compound

PFAINO927 / 150944

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.