MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DIAB Divinycell® F 90 Sandwich Core Material
Categories: Other Engineering Material; Composite Core Material; Polymer

Material Notes: Divinycell F is a recyclable, prepreg compatible sandwich core offering excellent FST (fire, smoke and toxicity) properties, good mechanicals and processing characteristics. Divinycell F has been specifically developed for commercial aircraft interior applications. It more than exceeds the US and European regulatory requirements for commercial aircraft interiors. Other key features include 220°C (425°F) processing temperature, superior damage tolerance, exceptional fatigue life, low water absorption, good chemical resistance and excellent heat aging at 180°C (356°F). Divinycell F is compatible with most common composite manufacturing processes. In addition, Divinycell F is both hot and cold formable.

    Resin Compatibility
  • Epoxy - Excellent
  • Phenolic - Very good with modern low free phenol resins
  • Cyanate Ester - Excellent
  • BMI - Sealer required
  • Polyester - Excellent
  • Vinylester - Excellent

Information Provided by DIAB

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0900 g/ccASTM D1622
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 2.15 MPaASTM D1623
Elongation at Break 60 %In Shear; ASTM C273
Compressive Strength 0.600 MPa
@Temperature 180 °C
ASTM D1621
 0.700 MPa
@Temperature 23.0 °C
ASTM D1621
Compressive Modulus 35.0 MPa
@Temperature 180 °C
ASTM D1621B
 40.0 MPa
@Temperature 23.0 °C
ASTM D1621B
Poissons Ratio 0.32
Shear Modulus 0.00950 GPaASTM C273
Shear Strength 1.10 MPaASTM C273
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 1.4
@Frequency 9.375e+9 Hz
ASTM D2520-01A
Dissipation Factor 0.0012
@Frequency 9.375e+9 Hz
ASTM D2520-01A
 
Thermal PropertiesOriginal ValueComments
CTE, linear 20.0 µin/in-°FASTM D696
Maximum Service Temperature, Air 180 °CExcellent Heat Aging; Continuous Service
Minimum Service Temperature, Air -100 °CContinuous
 
Descriptive Properties
Water Absorption (kg/m2)0.002ASTM D2842

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DIAB Divinycell® F 50 Sandwich Core Material
DIAB Divinycell® F 130 Sandwich Core Material
DIAB Divinycell® H 130 Sandwich Core Material
DIAB Divinycell® H 250 Sandwich Core Material
DIAB Divinycell® P 100 Sandwich Core Material

PDIAA934 / 99172

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.