MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
LG Chemical LUSEP HN2300W PPA+PTFE+GF30%, Injection Molding
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), Glass/PTFE Filled

Material Notes: Low friction, High temperature, High stiffness

Application: Automotive, E&E Part

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.48 g/ccASTM D792
Moisture Absorption 0.20 %
@Time 86400 sec
50% RH; ASTM D570
Linear Mold Shrinkage, Flow 0.0026 cm/cm
@Thickness 2.00 mm
ASTM D955
Linear Mold Shrinkage, Transverse 0.0069 cm/cm
@Thickness 2.00 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 170 MPa
@Thickness 3.20 mm
5mm/min; ASTM D638
Elongation at Break 2.1 %
@Thickness 3.20 mm
5mm/min; ASTM D638
Flexural Strength 240 MPa
@Thickness 3.20 mm
1.3mm/min; ASTM D790
Flexural Modulus 94800 kg(f)/cm²
@Thickness 3.20 mm
1.3mm/min; ASTM D790
Izod Impact, Notched 6.63 kg-cm/cm
@Thickness 3.20 mm
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmASTM D257
Dielectric Strength 23.0 kV/mm
@Thickness 1.00 mm
ASTM D149
 
Thermal PropertiesOriginal ValueComments
Melting Point 305 °CASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 280 °C
@Thickness 6.40 mm
Unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 300 - 320 °C
Middle Barrel Temperature 310 - 330 °C
Front Barrel Temperature 310 - 330 °C
Nozzle Temperature 320 - 340 °C
Melt Temperature 310 - 315 °C
Mold Temperature 100 - 140 °C
Drying Temperature 100 - 120 °C
@Time 14400 - 18000 sec
Moisture Content 0.060 - 0.10 %
Back Pressure 150 - 300 MPa
Screw Speed 50 - 150 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLHCHEM9840 / 239356

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.