MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Nucrel® 0910HS-SR Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating  (discontinued **)
Categories: Polymer; Thermoplastic; Ethylene Methyl Acrylate; Ethylene-Methyl Acrylate Copolymer, Coating Grade

Material Notes: 8.7 wt% Methacrylic Acid.

Nucrel® 0910HS-SR is an ethylene-methacrylic acid copolymer resin available for use in conventional and coextrusion coating equipment designed to process polyethylene resins.

Features/Benefits vs. Nucrel® 0910HS: Slip additives are added to reduce the coefficient of friction of the film surface to increase operating speeds on packaging machinery. Chill roll release agents are added to enhance extrusion coating speeds by reducing tendency of the hot melt to adhere to the chill roll surface

Typical Applications: Medical/pharmaceutical packaging; Condiment and miscellaneous nonfood pouches; Snack structures; Heat seal applications using vertical form-fill-seal packaging machinery.

Information provided by DuPont Packaging Polymers.

This product line/trade name was acquired by Dow, but this specific grade was discontinued prior to the acquisition.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.930 g/ccASTM D792
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Seal Strength 1500 g/25 mmseal bar 140°C.
Hot Tack Strength 1000 g/25 mmseal bar 110°C; DuPont Spring Test Method
 
Thermal PropertiesOriginal ValueComments
Melting Point 84.0 °CFreezing Point via DSC/ASTM D3418
 103 °CUpon Melting via DSC/ASTM D3418
Vicat Softening Point 86.0 °CASTM D1525
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 290 °CTypical Die Temp.
Melt Temperature 260 - 305 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Nucrel® 0411HS Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating
DuPont Elvaloy® 1126 AC Ethylene and 25% Methyl Acrylate Copolymer
Dow Nucrel® 0609HSA Ethylene-Methacrylic Acid Copolymer Resin for Film and Extrusion Coating/Laminating
Dow Nucrel® 403 Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
Dow Nucrel® 599 Ethylene-Methacrylic Acid Copolymer Resin

PDUPJC / 33646

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.