MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Azoty Tarnow™ Tarnamid® T-27 GF10 MX6 Polyamide 6 - Flame Retarded, Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass Fiber Filled, Flame Retardant

Material Notes: Flame retarded grade, reinforced with 10% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning, good surface quality.

Tarnamid® has the following main properties:

  • High mechanical strength, rigidity and hardness
  • High impact strength
  • High vibration damping capacity
  • Good fatigue strength
  • Very good sliding properties, abrasion resistance, low coefficient of friction
  • High thermal resistance, admissible temperature of continuous operation from -60°C to +150°C
  • High chemical resistance, particularly to organic solvents, oils, lubricants and fuels
  • Considerable moisture absorption influencing mechanical and electrical properties
  • Self-extinguishing properties (fire retardant properties)
  • Good electro-insulating properties
  • Good optical properties, relatively good transparency of molded pieces with thickness below 3.2 mm made from natural Tarnamid® (not dyed and not compounded)
  • Can be used for the production of goods coming into contact with food (grades fulfilling requirement of European Union Directive No 2002/72/EEC) with latest amendments

Information provided by Azoty Tarnow™.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.42 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0040 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0080 cm/cmISO 294-4
Melt Flow 35 g/10 min
@Load 5.00 kg,
Temperature 275 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 220 MPa
@Load 36.5 kg
ISO 2039-1
Tensile Strength 95.0 MPaISO 527
Elongation at Break 3.0 %ISO 527
Tensile Modulus 7.00 GPaISO 527
Flexural Strength 140 MPaISO 178
Charpy Impact Unnotched 40.0 kJ/m²ISO 179 1eU
Charpy Impact, Notched 3.50 kJ/m²ISO 179 1eA
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1.00e+15 ohmIEC 93
Dielectric Strength 28.0 kV/mmIEC 243-1
Comparative Tracking Index 600 VIEC 112
 
Thermal PropertiesOriginal ValueComments
Melting Point 221 °C
Deflection Temperature at 1.8 MPa (264 psi) 185 °CISO 75
Vicat Softening Point 200 °C
@Load 5.10 kg
ISO 306
Minimum Service Temperature, Air -60.0 °C
Flammability, UL94 V-2
@Thickness 1.60 mm
Glow Wire Flammability Index 960 °C
@Thickness 2.00 mm
PN-EN-60695-2-12
 
Processing PropertiesOriginal ValueComments
Melt Temperature 230 - 290 °C
Mold Temperature 60.0 - 120 °C80 - 90°C is recommended
Drying Temperature 75.0 - 100 °C
@Time 7200 - 14400 sec
Moisture Content <= 0.10 %
Injection Pressure 80.0 - 130 MPa80 MPa is recommended

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Azoty Tarnow™ Tarnamid® T-27 GF10 MX10 Polyamide 6 - Flame Retarded, Reinforced
Azoty Tarnow™ Tarnamid® T-27 GF15 Polyamide 6 - Glass Fiber Reinforced
Celanese Zytel® 70G13HS1L BK031 PA66-GF13
Lehvoss LUVOCOM® 1-8181 Polyamide 66 with carbon fiber, toughness-modified
Beijing Chemical Industry KAIFA® HN301-G10 PA6 Resin

PZAK925 / 121877

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.