MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Zirconium Orthosilicate, ZrSiO4 (Zircon)
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: White Tetragonal Crystals; other colors are possible depending on impurities present. Zircon crystals are sometimes cut as gemstones, not to be confused with popular diamond substitute cubic zirconia.

Key Words: ZrSiO4
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 4.60 g/cc
Molecular Weight 183.308 g/mol
 
Mechanical PropertiesOriginal ValueComments
Hardness, Mohs 7.5
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.5384 J/g-°CCrystal
Heat of Formation -2033.4 kJ/molCrystal
Decomposition Temperature 1540 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.94na
 1.99nß
 
Descriptive Properties
CAS Number10101-52-7
Mineral NameZircon
SolubilityInsoluble in H2O and Acid

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Anderman Ceramics EZZ 66P Zircon
Goodfellow Leachable Ceramic (Silica, Zircon, Alumina)
Reade Advanced Materials Zirconium Silicate (Zircon) Powder (ZrSiO4)
Accuratus MACOR Machinable Glass Ceramic
Zirconium Oxide, Zirconia, ZrO2

EINOR3398 / 5479

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.