Data provided by the manufacturer, Exxon Chemical. A 5.0% vinyl acetate copolymer clarity film resin. This resin's low melt index and its comonomer contact combine to provide film of special toughness and impact resistance as well as good heat sealability and low temperature properties. Applications: Frozen food packaging; Other food packaging including heavy duty produce bags, poultry bags, etc.; Packaging applications requiring good toughness and good heat sealability. Data for film properties below based on 1.25 mil film. |
Ethylene Vinyl Acetate; Exxon Chemical Company |