System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Petropol Makropol® B3 HV UV CRLA010 PC341 PC
Categories:
Polymer
;
Thermoplastic
;
Polycarbonate (PC)
;
Polycarbonate, Extruded
Material Notes:
Polycarbonate crystal, high viscosity, UV stabilized, excellent thermal and mechanical properties. Suitable for extrusion of multi wall sheet/profile.
Information provided by Petropol
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.20
g/cc
ISO 1183
Water Absorption
0.12 %
Humidity Absorption; ISO 62
Linear Mold Shrinkage, Flow
0.0060
cm/cm
ISO 2577
Linear Mold Shrinkage, Transverse
0.0080
cm/cm
ISO 2577
Melt Flow
>=
6.5
g/10 min
@Load 1.20 kg,
Temperature 300 °C
ISO 1133
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
65.0
MPa
50 mm/min; ISO 527-1/-2
Tensile Strength, Yield
67.0
MPa
50 mm/min; ISO 527-1/-2
Elongation at Break
100 %
50 mm/min; ISO 527-1/-2
Elongation at Yield
6.5 %
50 mm/min; ISO 527-1/-2
Tensile Modulus
2400
MPa
1 mm/min; ISO 527-1/-2
Flexural Strength
100
MPa
2 mm/min; ISO 178
Flexural Modulus
2400
MPa
2 mm/min; ISO 178
Izod Impact, Notched (ISO)
12.0
kJ/m²
@Temperature -30.0 °C
ISO 180/A
80.0
kJ/m²
@Temperature 23.0 °C
ISO 180/A
Charpy Impact Unnotched
14.0
kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
70.0
kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Tensile Creep Modulus, 1 hour
2200
MPa
ISO 899-1
Tensile Creep Modulus, 1000 hours
1900
MPa
ISO 899-1
Electrical Properties
Original Value
Comments
Volume Resistivity
1.00e+14
ohm-cm
IEC 60093
Surface Resistance
1.00e+16
ohm
IEC 60093
Dielectric Constant
3.0
@Frequency 1e+6 Hz
IEC 60250
3.1
@Frequency 100 Hz
IEC 60250
Dielectric Strength
34.0
kV/mm
@Thickness 1.00 mm
IEC 60243-1
Thermal Properties
Original Value
Comments
CTE, linear
0.650
µm/m-°C
ISO 11359-1,-2
Thermal Conductivity
0.200
W/m-K
ISO 8302
Deflection Temperature at 0.46 MPa (66 psi)
137
°C
ISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi)
126
°C
ISO 75-1,-2
Vicat Softening Point
144
°C
@Load 5.10 kg
50 °C/h; ISO 306
145
°C
@Load 5.10 kg
120 °C/h; ISO 306
Flammability, UL94
HB
@Thickness 0.750 mm
Glow Wire Test
850
°C
@Thickness 2.00 mm
IEC 60695-2-12
960
°C
@Thickness 3.00 mm
IEC 60695-2-12
Optical Properties
Original Value
Comments
Haze
>= 0.80 %
@Thickness 3.00 mm
ISO 14782
Transmission, Visible
>= 87 %
@Thickness 4.00 mm
ISO 13468-2
89 %
@Thickness 2.00 mm
ISO 13468-2
Processing Properties
Original Value
Comments
Processing Temperature
260
-
300
°C
Molding
Mold Temperature
60.0
-
100
°C
Drying Temperature
120
°C
Dry Time
4.00
hour
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PPETROPOL052 / 312960
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.