MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Schunk FE679PS Electrographite Salt Impregnated
Categories: Carbon; Graphite

Material Notes: Typical Application Fields: Dry running vanes subjected to high rotational speed.

Information provided by Schunk Graphite Technology, LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 2.20 g/cc0.0795 lb/in³
Porosity 2.0 %2.0 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 95955/62.5
Modulus of Elasticity 20.0 GPa2900 ksi
Flexural Strength 90.0 MPa13100 psi
Compressive Strength 210 MPa30500 psi
 
Thermal PropertiesMetricEnglishComments
CTE, linear  4.10 µm/m-°C
@Temperature 20.0 - 200 °C
2.28 µin/in-°F
@Temperature 68.0 - 392 °F
 5.20 µm/m-°C
@Temperature 200 - 600 °C
2.89 µin/in-°F
@Temperature 392 - 1110 °F
Thermal Conductivity 45.0 W/m-K312 BTU-in/hr-ft²-°F
 
Descriptive Properties
Inert Atmosphere800°C
Oxidizing Atmosphere500°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Graphite, Carbon, C
BACT Metal-Dylyn® Diamond-Like Nanocomposite Coating
BACT Dylyn® Diamond-Like Nanocomposite Coating
BACT DLC Diamond-Like Coating
Aremco Pyro-Paint™ 634-GR High Temperature Refractory Coating, GR >95%

CSCHU026 / 194783

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.