MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Poly Alloy Etoma™ ET1107 PP with Carbon Black
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with Carbon Black Filler

Material Notes: Etoma ET1107 resin is a conductive compound based on polypropylene with carbon black. ET1107 resin has not only stable surface resistivity but high impact property. It was designed to general purpose application which can be molded to big container or very small part.

Information provided by Poly Alloy Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.02 g/ccASTM D792
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 270 kg(f)/cm²ASTM D638
Elongation at Break 7.0 %ASTM D638
Flexural Strength 6400 psiASTM D790
Flexural Modulus 17500 kg(f)/cm²ASTM D790
Izod Impact, Notched 15.0 kg-cm/cmASTM D256
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square <= 1000 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 200 - 210 °C
Middle Barrel Temperature 200 - 220 °C
Front Barrel Temperature 205 - 225 °C
Nozzle Temperature 205 - 225 °C
Mold Temperature 30.0 - 65.0 °C
Drying Temperature 120 °C
Dry Time 4.00 - 8.00 hour
Shelf Life 24.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPALLOY020 / 278299

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.