MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Tra-Con Tra-Cast FS300 Thermally Conductive Electrically Insulating Compound
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-CAST FS300 is a medium viscosity, electrical insulating epoxy casting compound that is used for staking and setting transistors, diodes, resistors, integrated circuits and other heat sensitive components in printed circuit electronic applications. This two-part epoxy compound develops strong, durable high impact bonds at room temperature which improve heat transfer while maintaining electrical insulation. TRA-CAST FS300 bonds readily to itself, and to metals, silica, steatite, alumina, sapphire and other ceramics, glass, plastics and many other materials because its coefficient of thermal expansion provides a good match for those materials over a fairly wide temperature range. Fuly cured TRA-CAST FS300 provides excellent resistance to salt solutions, mild acids and alkalis, and many other chemicals including petroleum solvents, lubricating oils, and alcohol.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.52 g/cc1.52 g/ccMixed
Solids Content 100 %100 %Reactive Solids Content
Viscosity 6000 cP
@Temperature 25.0 °C
6000 cP
@Temperature 77.0 °F
After mixing
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 9090
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.00e+15 ohm-cm3.00e+15 ohm-cm
 2.00e+13 ohm-cm
@Temperature 75.0 °C
2.00e+13 ohm-cm
@Temperature 167 °F
Dielectric Constant 5.9
@Frequency 1000 Hz
5.9
@Frequency 1000 Hz
Dielectric Strength 16.1 kV/mm410 kV/in
Dissipation Factor 0.010
@Frequency 1000 Hz
0.010
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 28.0 µm/m-°C
@Temperature 20.0 °C
15.6 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 0.840 W/m-K5.83 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 120 °C248 °F
Minimum Service Temperature, Air -70.0 °C-94.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 360 min6.00 hour4 hrs @ 25°C + 2 hrs @ 65°C
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Pot Life 120 min120 min
 
Descriptive Properties
Color Black
Mix Ratio, parts by weight100/52Resin/Hardener

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tra-Con Tra-Bond 2151 Thermally Conductive Electrically Insulating Compound
Tra-Con Supertherm 816H01 Thermally Conductive Electrically Insulating Compound
Momentive Performance Materials TSE3331 Dark Gray Thermally Conductive Potting/Encapsulating Compound
Tra-Con Tra-Bond 2159 Heat Conductive Electrically Insulating Compound
Tra-Con Tra-Bond 2158 Heat Conductive Electrically Insulating Compound

PTRAC278 / 71206

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.