MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for T 300 Series Stainless Steel
Categories: Metal; Ferrous Metal; Stainless Steel; T 300 Series Stainless Steel

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "T 300 Series Stainless Steel". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.190 - 9.01 g/ccAverage value: 7.85 g/cc Grade Count:411
Porosity 1.00 - 5.00 %Average value: 3.83 % Grade Count:6
Particle Size 6.70 - 300 µmAverage value: 28.1 µm Grade Count:29
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 80.0 - 382Average value: 188 Grade Count:165
Hardness, Knoop 97.0 - 414Average value: 202 Grade Count:80
Hardness, Rockwell B 37.0 - 100Average value: 82.2 Grade Count:215
Hardness, Rockwell C 15.0 - 43.0Average value: 29.0 Grade Count:28
Hardness, Vickers 82.0 - 400Average value: 197 Grade Count:90
Tensile Strength, Ultimate 34.5 - 2200 MPaAverage value: 703 MPa Grade Count:488
Tensile Strength, Yield 138 - 1800 MPaAverage value: 420 MPa Grade Count:458
Elongation at Break 1.00 - 88.0 %Average value: 33.1 % Grade Count:466
Elongation at Yield 28.0 - 62.0 %Average value: 39.1 % Grade Count:7
Reduction of Area 35.0 - 88.0 %Average value: 53.3 % Grade Count:78
Modulus of Elasticity 79.3 - 220 GPaAverage value: 195 GPa Grade Count:349
Compressive Yield Strength 262 - 1320 MPaAverage value: 707 MPa Grade Count:5
Poissons Ratio 0.240 - 0.340Average value: 0.285 Grade Count:128
Fatigue Strength 180 - 605 MPaAverage value: 369 MPa Grade Count:19
Shear Modulus 70.3 - 86.0 GPaAverage value: 77.6 GPa Grade Count:141
Izod Impact 55.0 - 165 JAverage value: 133 J Grade Count:106
Izod Impact Unnotched 108 - 149 JAverage value: 130 J Grade Count:7
Charpy Impact 43.0 - 325 JAverage value: 156 J Grade Count:114
Charpy Impact, Unnotched 190 - 216 JAverage value: 198 J Grade Count:3
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000695 - 0.000108 ohm-cmAverage value: 0.0000764 ohm-cm Grade Count:303
Magnetic Permeability 1.00 - 8.48Average value: 1.28 Grade Count:175
Curie Temperature -115 °CAverage value: -115 °C Grade Count:7
 
Thermal PropertiesOriginal ValueComments
CTE, linear 13.4 - 20.5 µm/m-°CAverage value: 17.5 µm/m-°C Grade Count:291
Specific Heat Capacity 0.450 - 0.502 J/g-°CAverage value: 0.497 J/g-°C Grade Count:294
Thermal Conductivity 11.6 - 22.6 W/m-KAverage value: 15.3 W/m-K Grade Count:172
Melting Point 1230 - 1510 °CAverage value: 1410 °C Grade Count:265
Solidus 1230 - 1450 °CAverage value: 1390 °C Grade Count:262
Liquidus 1390 - 1510 °CAverage value: 1430 °C Grade Count:262
Maximum Service Temperature, Air 260 - 1150 °CAverage value: 922 °C Grade Count:149
Minimum Service Temperature, Air -200 - -196 °CAverage value: -197 °C Grade Count:6
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 1010 - 1090 °CAverage value: 1050 °C Grade Count:4
Hot-Working Temperature 899 - 1290 °CAverage value: 1120 °C Grade Count:6
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.100 - 0.800 %Average value: 0.323 % Grade Count:15
Carbon, C 0.0100 - 0.750 %Average value: 0.0857 % Grade Count:523
Chromium, Cr 12.5 - 57.0 %Average value: 19.6 % Grade Count:530
Cobalt, Co 0.0500 - 0.200 %Average value: 0.189 % Grade Count:14
Copper, Cu 0.200 - 5.00 %Average value: 1.13 % Grade Count:50
Iron, Fe 5.50 - 78.0 %Average value: 64.2 % Grade Count:525
Manganese, Mn 0.100 - 6.00 %Average value: 1.87 % Grade Count:522
Molybdenum, Mo 0.300 - 7.90 %Average value: 2.72 % Grade Count:177
Nb + Ta 0.800 - 1.10 %Average value: 0.843 % Grade Count:40
Nickel, Ni 3.00 - 39.0 %Average value: 13.0 % Grade Count:530
Niobium, Nb (Columbium, Cb) 0.100 - 1.00 %Average value: 0.708 % Grade Count:19
Nitrogen, N 0.00500 - 1.00 %Average value: 0.153 % Grade Count:104
Oxygen, O 0.250 %Average value: 0.250 % Grade Count:4
Phosphorus, P 0.00700 - 0.450 %Average value: 0.0485 % Grade Count:469
Selenium, Se 0.150 - 0.350 %Average value: 0.175 % Grade Count:4
Silicon, Si 0.0500 - 3.00 %Average value: 1.01 % Grade Count:521
Sulfur, S 0.00100 - 0.400 %Average value: 0.0368 % Grade Count:474
Tantalum, Ta 0.100 - 1.00 %Average value: 0.250 % Grade Count:18
Tin, Sn 2.00 %Average value: 2.00 % Grade Count:9
Titanium, Ti 0.0100 - 2.35 %Average value: 0.415 % Grade Count:24
WC 0.0450 %Average value: 0.0450 % Grade Count:4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for T 400 Series Stainless Steel
Overview of materials for Stainless Steel
Overview of materials for T S10000 Series Stainless Steel
Overview of materials for T 600 Series Stainless Steel
303 Stainless Steel, annealed

M01024 / 81735

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.