MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Monmouth Rubber & Plastics Durafoam™ P493SHD EPDM
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Note 1: The Durafoam™100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from ¼ inch thick sheets. These test pieces were exposed for 120 hours to a cycle consisting of:
1. Light at 70°C for 8 hours
2. Dark at 50° C for 4 hours
3. Condensation Cooling for 15 minutes

Information provided by Monmouth Rubber & Plastics Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 15.0 lb/ft³
Water Absorption <= 5.0 %ASTM D1056
Linear Mold Shrinkage <= 0.017 cm/cmNote 1
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 110 psi
Elongation at Break >= 200 %
Compressive Strength 9.00 - 13.0 psi25%
Compression Set <= 25 %B2 – 50%
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 300 °F
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Vicone High Performance Rubber VicoSeal™ 617N-BK Rubber Vulcanized to SS304
3M 5690K Silicone Rubber Termination Kits
3M 5600 Cold Shrink Silicone Rubber Termination Kits QT-III
3M 4605 Silicone Rubber Termination Kit
Precision Polymer Engineering R60R Natural Rubber

PMONM024 / 160826

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.