Product Description Grilamid L 20 H FWA black 9225 is a medium viscosity, unreinforced and heat stabilized Polyamide 12 (PA12). Grilamid L 20 H FWA black 9225 is used for technical injection molded parts, and is in particular suitable for parts with low to medium wall thicknesses. This material allows further the molding of thick articles with walls up to 15 mm.- high impact strength
- high elongation at break
- very low moisture absorption
- good chemical resistance
- easy processing
- low density
The particular stabilization package of Grilamid L 20 H FWA black 9225 allows the use in direct contact with potable water and foodstuff.Information provided by EMS Grivory. |