Product: PLEXIGLAS® Film 0F058 is an amorphous thermoplastic film based on polymethyl methacrylate (PMMA). Properties: PLEXIGLAS® Film 0F058 provides an excellent light transmission and brilliance due to a low intrinsic absorption. Based on the very good optical density of PLEXIGLAS® Film 0F058, a high luminous efficiency can be achieved even at very long distances. The film is manufactured in a calendar process with a polishing stack technology. Therefore, PLEXIGLAS® Film 0F058 provides a high gloss surface on both sides. Application: PLEXIGLAS® Film 0F058 is used as light guide film in electronic devices. The former Evonik Methacrylates business has been sold to Röhm GmbH (Roehm). |