MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Redwood Plastics TIVAR® 88 & 88-2 UHMW
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: A premium lining material for bulk material handling, Redco™ Tivar® 88 promotes flow of cohesive or non-free flowing materials due to its low surface friction. Redco™ Tivar® 88 liners are the perfect solution to reduce or eliminate arching, ratholing and erratic material flow challenges.

Standard Color: Blue, White & Black

Fusion welded Redco™ UHMW sheets are available to eliminate lifting; up to 144” x 1200”.

Typical Applications: Belt skirting, chute liners, conveying components, bearings, belt guides, chain guides, curves, guide rails, wear strip, dead plates, diverter bars, guide rollers, hitch plates, hopper liners, liners for gravity flow applications, roller covers, transfer plates, under belt wear strips, belt scrapers, bunker liners, chain conveyor flights, chute liners, conveyor skirting, cyclones, drag chain conveyor liners, dragline buckets, dust collection hopper liners, front end loader bucket liners, hopper liners, off-road truck beds, truck bed lining for asphalt hauling, pugmill paddles, railcar liners, reclaimer buckets, screw conveyor liners, self-unloading ships, silo liners, slider beds, storage bin liners surge bin liners, transfer chute liners, under chain guides, vibrating bin, dischargers, vibratory feeder liners, etc.

Information provided by Redwood Plastics and Rubber

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.930 g/ccASTM D 792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 69ASTM D 2240
Tensile Strength at Break 5600 psiASTM D638
Tensile Strength, Yield 3000 psiASTM D638
Elongation at Break 300 %ASTM D 638
Tensile Modulus 102000 psiASTM D638
1% Secant Modulus 102000 psiASTM D790B
Izod Impact, Notched NBASTM D256A
Coefficient of Friction, Static 0.12(DRY vs. STEEL)
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+17 ohm-cmASTM D 257
Surface Resistance 1.00e+17 ohmASTM D 257
Dielectric Constant 2.3ASTM D 150
Dissipation Factor <= 0.00050ASTM D 150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 20.0 µm/m-°C
@Temperature -30.0 - 60.0 °C
ASTM D-2240
Maximum Service Temperature, Air 180 °FConstant
 200 °FIntermittent
 
Descriptive Properties
FDA ()NO

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PREDW012 / 296578

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.