MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Crucible Steel CPM® Rex M4 HC(HS) Tool Steel
Categories: Metal; Ferrous Metal; Carbon Steel; High Carbon Steel; Tool Steel

Material Notes: CPM REX M4 HC(HS) is a high vanadium special purpose high speed steel exhibiting better wear resistance and toughness than M2 or M3 in cold work punches, die inserts and cutting applications involving high speed and light cuts.

The high carbon (HC) modification to standard M4 is designed to provide optimum hardening response in larger cross-section tools or in vacuum or atmosphere heat treating.

The high sulfur (HS) modification is standard for larger diameter bars, providing enhanced machinability and grindability.

The CPM process produces very homogeneous, high quality steel characterized by superior dimensional stability, grindability, and toughness compared to steels produced by conventional processes.

Information provided by Crucible Specialty Metals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.97 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 225 - 255Annealed
Hardness, Rockwell C 63.5Hardening Temperature- 1165°C; Tempering Temperature- 565°C
 65.5Hardening Temperature- 1205°C; Tempering Temperature- 550°C
Modulus of Elasticity 214 GPa
Flexural Strength 5088 MPaHardening Temperature- 1205°C, Tempering Temperature- 550°C
 5129 MPaHardening Temperature- 1165°C, Tempering Temperature- 565°C
Charpy Impact 27.0 JHardening Temperature- 1205°C; Tempering Temperature- 550°C
 38.0 JHardening Temperature- 1165°C; Tempering Temperature- 565°C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.5 µm/m-°C
@Temperature 40.0 - 260 °C
 12.1 µm/m-°C
@Temperature 40.0 - 540 °C
Thermal Conductivity 18.99 W/m-K
 20.82 W/m-K
@Temperature 100 °C
 23.96 W/m-K
@Temperature 300 °C
 25.58 W/m-K
@Temperature 500 °C
 26.09 W/m-K
@Temperature 540 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 1.42 %
Chromium, Cr 4.0 %
Iron, Fe 79.47 %As Remainder
Magnesium, Mg 0.30 - 0.70 %
Molybdenum, Mo 5.25 %
Sulfur, S 0.060 - 0.22 %
Tungsten, W 5.5 %
Vanadium, V 4.0 %
 
Descriptive Properties
Grindability; Metal Removed/Wheel Worn4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Crucible Steel REX® M4 High Speed Steel
AISI Type M4 Molybdenum High Speed Tool Steel (UNS T11304)
Carpenter Four Star High Speed Steel Red-Wear® (AISI M4)
Crucible Steel CPM® 4V® Tool Steel
Bohler-Uddeholm BÖHLER S692/S693 MICROCLEAN® PM M4 High Speed Steel

NCRUC005 / 15998

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.