MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chi Mei Polylac® PA-777B ABS - High Heat
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded

Material Notes: High Heat Impact

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.03 g/cc0.0372 lb/in³ISO 1183
Linear Mold Shrinkage 0.0030 - 0.0070 cm/cm0.0030 - 0.0070 in/inASTM D955
Melt Flow 6.7 g/10 min
@Load 10.0 kg,
Temperature 220 °C
6.7 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO-1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 112112ASTM D785
Ball Indentation Hardness 91.0 MPa13200 psiH358/30; ISO 2039-1
Tensile Strength at Break 34.0 MPa4930 psi50 mm/min; ISO 527
Tensile Strength, Yield 45.0 MPa6530 psi50 mm/min; ISO 527
Elongation at Break 18 %18 %50 mm/min; ISO 527
Flexural Strength 70.0 MPa10200 psi2 mm/min; ISO 178
Flexural Modulus 2.20 GPa319 ksi2 mm/min; ISO 178
Izod Impact, Notched  2.05 J/cm
@Thickness 6.35 mm
3.84 ft-lb/in
@Thickness 0.250 in
ASTM D256
 2.38 J/cm
@Thickness 3.17 mm
4.46 ft-lb/in
@Thickness 0.125 in
ASTM D256
Izod Impact, Notched (ISO) 19.0 kJ/m²9.04 ft-lb/in²ISO 180/1A
Izod Impact, Unnotched (ISO) NBNBISO 180/1C
Charpy Impact Unnotched NBNBISO 179
Charpy Impact, Notched 2.00 J/cm²9.52 ft-lb/in²ISO 179
Impact 1414Impact Flexural Test Notched (KJ/m²)
 NBNBImpact Flexural Test Unnotched (KJ/m²)
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C203 °Funannealed; ISO 75
 105 °C221 °Fannealed; ISO 75
Vicat Softening Point  105 °C
@Load 5.00 kg
221 °F
@Load 11.0 lb
50°C/hr; ISO 306
 107 °C
@Load 5.00 kg
225 °F
@Load 11.0 lb
120°C/hr; ISO 306
 113 °C
@Load 1.00 kg
235 °F
@Load 2.20 lb
50°C/hr; ISO 306
 115 °C
@Load 1.00 kg
239 °F
@Load 2.20 lb
120°C/hr; ISO 306
Flammability, UL94 HB
@Thickness 1.59 mm
HB
@Thickness 0.0625 in
UL 94

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chi Mei Polylac® PA-777D ABS - High Heat
Chi Mei Polylac® PA-777E ABS - High Heat
Chi Mei Polylac® PA-765B ABS - Flame Retardant
Chi Mei Polylac® PA-727 ABS
Chi Mei Polylac® PA-747R ABS - Extrusion

PCHI927 / 109415

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.