MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Accella Bayblock® II/Base Acrylic Coating
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: Characterization: Bayblock II coating is a technologically advanced, high-solids, fire resistant, thixotropic, acrylic elastomeric coating.

Properties / Applications: Bayblock II coating is formulated for the protection of sprayed-in place polyurethane foam, stucco, cinder blocks, metal, single ply, and with appropriate base coats, asphaltic and modified bituminous roofing. As with any product, use of Bayblock II coating must be tested (including, but not limited to, field testing) in advance by the user to determine suitability.

Covestro sold their spray polyurethane foam business to Accella in 2017.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.44 g/cc0.0520 lb/in³
Solids Content 53 - 57 %53 - 57 %ASTM D6083, by volume
 68 - 72 %68 - 72 %ASTM D6083, by weight
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 1.92 MPa278 psiASTM D412
Elongation at Break 502 %502 %ASTM D412
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 93.3 °C200 °F
Minimum Service Temperature, Air -34.4 °C-30.0 °F
 
Descriptive Properties
ColorWhite, Tan, Gray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Schott N-FK51A Glass
Concrete, Cinder
Commercial Construction Brick

PCOVEST0061 / 201844

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.