Product Description: Styroflex® 4G80 is a styrene butadiene Block copolymer (SBC) optimized for extrusion. Features: Good kink resistance; Good transparency; Good solvent bonding; Soft feel surface Applications: Tubing for medical devices; Grips for tools or sports equipmentAvailability: Africa & Middle East; Europe; Latin America; North America Features: Block Copolymer; Bondability; High Clarity; Kink Resistant; Soft Uses: Flexible Grips; Medical/Healthcare Applications; Power/Other Tools; Sporting Goods; Tubing Appearance: Clear/Transparent Form: Pellets Processing Method: Extrusion Information provided by INEOS Styrolution |