MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sandvik 19.9.R-16 Covered electrodes
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Sandvik 19.9.R-16 (308/308H-16) is a covered chromium-nickel electrode with rutile-basic coating for welding of steels of ASTM 304 types as well as overlays giving 308 type composition. This electrode has the same composition as type 308 except the carbon restriction eliminates carbon content below 0.04%. Carbon content in the range 0.04-0.08 facilitates higher tensile and creep strengths at elevated temperatures. The coating for this electrode is of the American rutile type with a faster freezing rate over -17 Type of the same weld deposit chemistry. The electrode has excellent arc stability and fast burn off rate with minimal stub loss. It is also characterized by improved moisture resistance, self-peeling slag, easy post weld finishing. Sandvik 19.9.R-16 (308/308H-16) gives smooth uniform beads and works in any standard weld position.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 200200
Tensile Strength, Ultimate 620 MPa89900 psiRm
Tensile Strength, Yield 441 MPa
@Strain 0.2 %
64000 psi
@Strain 0.2 %
Elongation at Break 41 %41 %
Impact Test 122 J90.0 ft-lb
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.060 %0.060 %
Chromium, Cr 20.5 %20.5 %
Manganese, Mn 2.0 %2.0 %
Nickel, Ni 9.5 %9.5 %
Silicon, Si 0.60 %0.60 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NSANDV5299 / 199863

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.