MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Higun 175X Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Gun installation. Higun 175X is 3182°F (1750°C) grade low cement gunning material. Higun combines the superior physical properties of a low cement monolithic with the practical advantages of a gunning material. The Higun range of low cement gun mixes are designed to be installed with conventional gunning equipment with some accessories to maximize the product properties.

Applications:

  • Forge furnace hearths
  • Door jambs
  • Lintels and piers
  • Cartops
  • Rotary kiln nose rings, retainer rings and dams
  • Rotary hearth curbs
  • Walking beam furnace hearth
  • Pusher furnace hearths
  • Skid pipe protection
  • Troughs for molten copper

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.691 g/cc
@Temperature 816 °C
fired; ASTM C134
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 59.0 - 76.0 MPa
@Temperature 816 °C,
Time 18000 sec
fired, Cold Crushing Strength; ASTM C133
 69.0 - 97.0 MPa
@Temperature 1000 °C,
Time 18000 sec
fired, Cold Crushing Strength; ASTM C133
 76.0 - 103 MPa
@Temperature 1600 °C,
Time 18000 sec
fired, Cold Crushing Strength; ASTM C133
Abrasion 7.0 - 12
@Temperature 816 °C
cm3, fired; ASTM C704
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 1.90 W/m-K
@Temperature 600 °C
ASTM C201
Maximum Service Temperature, Air <= 1750 °C
Shrinkage 0.00 - 0.20 %
@Treatment Temp. 104 °C,
Time 86400 sec
dried
 0.20 %
@Treatment Temp. 816 °C,
Time 18000 sec
fired
 0.30 %
@Treatment Temp. 1000 °C,
Time 18000 sec
fired
 0.40 %
@Treatment Temp. 1600 °C,
Time 18000 sec
fired
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
 
Component Elements PropertiesOriginal ValueComments
Al2O3 81 %
CaO 2.8 %
Fe2O3 1.0 %
SiO2 13 %
 
Descriptive Properties
Placement, average (kg)73to place 1m3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CMORF6400 / 203184

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.