MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Chemlon® A40 Nylon 66, Dry, Heat Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Heat Stabilized

Material Notes: Notes: A30 is an unfilled injection molding grade of nylon 66. It contains a nucleating agent to enable moldings to be produced with shorter cycle times.

Availability: Europe

Additive: Heat Stabilizer

Features: Heat Stabilized

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ISO 1183
Moisture Absorption at Equilibrium 2.5 %2.5 %50% RH; ISO 62
Linear Mold Shrinkage 0.012 - 0.018 cm/cm0.012 - 0.018 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 75.2 MPa10900 psiISO 527-2
Tensile Modulus 2.90 GPa421 ksiISO 527-2
Flexural Strength 95.1 MPa13800 psiISO 178
Flexural Modulus 2.80 GPa406 ksiISO 178
Charpy Impact Unnotched NBNBISO 179/1eU
Charpy Impact, Notched 1.01 J/cm²4.80 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohm1.00e+14 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 220 °C428 °FUnannealed; ISO 72-2/B
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C194 °FUnannealed; ISO 72-2/A
Flammability, UL94 V-2
@Thickness 1.52 mm
V-2
@Thickness 0.0600 in
Oxygen Index 27 %27 %ISO 4589-2
Glow Wire Flammability Index 749 °C
@Thickness 1.52 mm
1380 °F
@Thickness 0.0600 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 270 - 290 °C518 - 554 °F
Middle Barrel Temperature 270 - 290 °C518 - 554 °F
Front Barrel Temperature 270 - 290 °C518 - 554 °F
Melt Temperature 270 - 290 °C518 - 554 °F
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 80.0 °C176 °F
Dry Time 2.00 hour2.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ0542 / 237033

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.