MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Mitsubishi Chemical Advanced Materials Ertalon® LFX PA 6 + oil, cast (ISO Data)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Cast

Material Notes: This internally lubricated cast nylon 6 is self-lubricating in the real meaning of the word. Ertalon LFX, especially developed for unlubricated, highly loaded and slow moving parts applications, yields a considerable enlargement of the application opportunities compared to standard cast nylons. It offers a reduced coefficient of friction (up to 50% lower), considerably increasing the pressure-velocity capabilities, and a vastly improved wear resistance (up to 10 times better).

  • High mechanical strength, stiffness, hardness and toughness
  • Good fatigue resistance
  • High mechanical damping ability
  • Good sliding properties
  • Excellent wear resistance
  • Good electrical insulating properties
  • Good resistance to high energy radiation (gamma- and X-rays)
  • Good machinability

Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.135 g/cc0.04100 lb/in³ISO 1183-1
Moisture Absorption at Equilibrium 2.0 %2.0 %50% RH
Water Absorption at Saturation 6.3 %6.3 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8282ISO 2039-2
Hardness, Shore D 7676
Ball Indentation Hardness 145 MPa21000 psiISO 2039-1
Tensile Strength, Yield 73.0 MPa10600 psiISO 527-1/-2
Elongation at Break 25 %25 %ISO 527-1/-2
Elongation at Yield 5.0 %5.0 %ISO 527-1/-2
Tensile Modulus 3.00 GPa435 ksiISO 527-1/-2
Flexural Strength 107 MPa15500 psi
Flexural Modulus 3.00 GPa435 ksi
Compressive Strength  31.0 MPa
@Strain 1 %
4500 psi
@Strain 1 %
ISO 604
 58.0 MPa
@Strain 2 %
8410 psi
@Strain 2 %
ISO 604
 85.0 MPa
@Strain 5.0 %
12300 psi
@Strain 5.0 %
ISO 604
K Factor (ISO) 4.5 µm/km4.5 µm/km
Charpy Impact Unnotched 5.00 J/cm²23.8 ft-lb/in²ISO 179-1/1eU
Charpy Impact, Notched 0.400 J/cm²1.90 ft-lb/in²ISO 179-1/1eA
Coefficient of Friction, Dynamic 0.20 - 0.350.20 - 0.35
Limiting Pressure Velocity 0.150 MPa-m/sec4280 psi-ft/minat 1 m/s unlubricated
 0.230 MPa-m/sec6570 psi-ft/minat 0.1 m/s unlubricated
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.0e+14 ohm-cm>= 1.0e+14 ohm-cmIEC 60093
Surface Resistivity per Square >= 1.0e+13 ohm>= 1.0e+13 ohmIEC 60093
Dielectric Constant 3.5
@Frequency >=100000 Hz
3.5
@Frequency >=100000 Hz
IEC 60250
Dielectric Strength 22.0 kV/mm559 kV/in
Dissipation Factor 0.015
@Frequency 100000 Hz
0.015
@Frequency 100000 Hz
IEC 60250
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 90.0 µm/m-°C
@Temperature 23.0 - 100 °C
50.0 µin/in-°F
@Temperature 73.4 - 212 °F
Thermal Conductivity 0.280 W/m-K1.94 BTU-in/hr-ft²-°F
Melting Point 215 °C419 °FDSC, 10°C/min.; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 °C194 °FContinuous; 20,000 h
 105 °C221 °FContinuous; 5,000 h
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C167 °FISO 75-1/-2
Flammability, UL94 HBHB
 
Compliance PropertiesMetricEnglishComments
3A-Dairy NoNo
European Food 1935/2004 NoNo
FDA NoNo
USP Class VI NoNo
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) UnacceptableUnacceptable
Acids, Weak LimitedLimited
Alcohols LimitedLimited
Alkalies, Strong (pH 11-14) UnacceptableUnacceptable
Alkalies, Weak LimitedLimited
Chlorinated Solvents LimitedLimited
Continuous Sunlight LimitedLimited
Hot Water / Steam LimitedLimited
Hydrocarbons - Aliphatic AcceptableAcceptable
Hydrocarbons - Aromatic AcceptableAcceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters AcceptableAcceptable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Acetron® GP Copolymer Acetal, Porosity-Free, Unfilled, Extruded (ASTM datasheet)
Mitsubishi Chemical Advanced Materials Ertalon® 66 SA PA 66, extruded (ISO Data)
Overview of materials for Polytetrafluoroethylene (PTFE), Molded
Chemours Teflon® PTFE Grade K-10 Fluoropolymer Resin
Mitsubishi Chemical Advanced Materials Ertalon® 4.6 PA 4.6, extruded (ISO Data)

P1SMU836 / 130658

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.