MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Henkel Loctite® Stycast® ES 6005 Two-Component Epoxy Potting Compound
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Loctite Stycast ES 6005 provides the following product characteristics: Room temperature cure

Application: Potting and Encapsulating

Loctite Stycast ES 6005 is a resilient, low cost, fast gelling, potting compound. Designed for easy 2 to 1 meter mix- dispense machinery and low abrasion. This material is ideal for potting and encapsulating high volume parts.

UL Classification: Classified by Underwriters Laboratories Inc.® UL 1446 as a potting compound with and without varnish up to a temperature of 180 °C.

Information provided by Henkel.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.970 g/cc0.0350 lb/in³Part B
 1.41 g/cc0.0509 lb/in³Mixed
 1.63 g/cc0.0589 lb/in³Part A
Water Absorption 0.30 %
@Time 86400 sec
0.30 %
@Time 24.0 hour
ISO 62
Viscosity 170 cP170 cPPart B
 1500 cP1500 cPMixed
 11000 cP11000 cPPart A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7070ISO 868
Tensile Strength 12.4 MPa1800 psiISO 527-2
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 4.90e+13 ohm-cm4.90e+13 ohm-cmIEC 60093
Surface Resistance 5.40e+14 ohm5.40e+14 ohmIEC 60093
Dielectric Constant  4.5
@Frequency 100000 Hz
4.5
@Frequency 100000 Hz
IEC 60250
 5.0
@Frequency 1000 Hz
5.0
@Frequency 1000 Hz
IEC 60250
 5.2
@Frequency 100 Hz
5.2
@Frequency 100 Hz
IEC 60250
Dielectric Strength 38.0 kV/mm965 kV/inIEC 60243-1
Dissipation Factor  0.030
@Frequency 1000 Hz
0.030
@Frequency 1000 Hz
IEC 60250
 0.030
@Frequency 100000 Hz
0.030
@Frequency 100000 Hz
IEC 60250
 0.040
@Frequency 100 Hz
0.040
@Frequency 100 Hz
IEC 60250
Arc Resistance 87 sec87 secASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear  47.0 µm/m-°C
@Temperature <=14.0 °C
26.1 µin/in-°F
@Temperature <=57.2 °F
Pre Tg (Alpha 1); ASTM D7012
 167 µm/m-°C
@Temperature >=14.0 °C
92.8 µin/in-°F
@Temperature >=57.2 °F
Post Tg (Alpha 2); ASTM D7012
Thermal Conductivity 0.288 W/m-K2.00 BTU-in/hr-ft²-°FISO 8302
Glass Transition Temp, Tg 14.0 °C57.2 °FISO 11357-2
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Cure Time  120 min
@Temperature 66.0 °C
2.00 hour
@Temperature 151 °F
Alternate
 960 min
@Temperature 25.0 °C
16.0 hour
@Temperature 77.0 °F
Recommended
Pot Life 10.0 min10.0 min400 g mass
Gel Time 25.0 min25.0 min400 g mass
 
Descriptive Properties
AppearanceAmber - greenComponent B, Hardener
 BlackComponent A, Resin
Mix Ratio, by Volume2 : 1Part A : Part B
Mix Ratio, by Weight100 : 29.5Component A : Component B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHENK7954 / 255439

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.