MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Zoltek™ OX Continuous Tow Oxidized PAN Fiber
Categories: Carbon; Carbon Fiber/Carbon Fibre; Other Engineering Material; Composite Fibers

Material Notes: ZOLTEK OX continuous tow fibers are oxidized/stabilized PAN fibers (OPAN) that are inherently fire resistant, thermally stable, exhibit excellent resistance to chemicals and solvents and are electrically non-conductive. Available crimped or uncrimped, ZOLTEK OX continuous tow is suitable for stretch breaking into yarn, cutting into flock, crimping & cutting into staple fibers for nonwovens or yarn spinning.

Information provided by Zoltek Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.36 g/ccfiber
 1.37 g/ccstandard density
 1.40 g/cchigh density
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 240 - 300 MPaStandard and High density
Elongation at Break 22 - 28 %Standard and high density.
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 8.00e+8 ohm-cmStandard and high density.
 
Thermal PropertiesOriginal ValueComments
Oxygen Index >= 40 %Fiber property
 >= 45 %˜ 45. Standard Density
 >= 55 %˜ 55. High Density
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 62 %
Hydrogen, H 4.5 %
Nitrogen, N 21.5 %
O2 12 %
Sodium, Na <= 0.10 %
Trace Metals <= 0.010 %
 
Descriptive Properties
ColorBlack
Fiber Diameter (µm)12.5. High Density.
 12.5. Standard density.
 14. High Density.
 14. Standard density
 22. Standard density.
Filament Count160k. Standard density.
 300k. High density
 300k. Standard density.
Fineness ()1.7 dTexStandard Density
 1.7 dTexHigh Density
 2.2 dTexHigh Density
 2.2 dTexStandard Density
 5 dTexStandard Density
FormatUncrimped. Standard and high density.
Organic SolventsExcellent resistance
Strong AcidsGood resistance
Strong BasesPoor resistance
Weak AcidsExcellent resistance
Weak BasesGood resistance

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® HexTow® AS4 6K Standard Modulus Carbon Fiber (6000 Filaments)
Aremco Graphi-Bond™ 551-R
Graphite, Carbon, C
Hexcel® HexTow® AS4 12K Standard Modulus Carbon Fiber (12,000 Filaments)
Hexcel® HexTow® AS4 3K Standard Modulus Carbon Fiber (3000 Filaments)

ECZO826 / 232297

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.