MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
BASF 2,3,5-Trimethylhydroquinone
Categories: Fluid

Material Notes: Formula: C9H12O2

CAS: 700-13-0

Description: TMHQ is a colorless fine crystalline powder. It is insoluble in water, soluble in methanol, ethanol, diethyl ether, and acetone.

Synonyms: TMHQ, TMH

Applications: Intermediate used in the production of Synthesis processes.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.400 - 0.450 g/cc
Molecular Weight 152.2 g/mol
 
Thermal PropertiesOriginal ValueComments
Melting Point 169 - 172 °C
Flash Point 191 °C
Ignition Temperature 405 °C
 
Descriptive Properties
Assay>99.5%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF DEHA DI-2-Ethylhexylamine
BASF D 2000 Polyetheramine
BASF Cetyl Chloroformate
BASF Butanediol Divinyl Ether
BASF AH-Salt

PBASG1053 / 132686

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.