MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M 5680 Cold Shrink Silicone Rubber Termination Kits QT-III
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: 3M™ Cold Shrink 5600 and 5680 Series QT-II Termination Kits contain one-piece silicone rubber terminations designed for concentric neutral (CN) cable. They meet the requirements of IEEE 48-1990 for Class I termination. In addition, they meet German standard VDA 0278 parts 5 & 100, British standard BS C-89, Spanish standard UNE 21-115-75 and Brazilian standard A-B-N-T-9314. Similar terminations using Cold Shrink technology meet French EdF standards HN 33-E-01. Data on foreign standards are available upon request. The 3M termination consists of a high dielectric constant (Hi-K) stress control tube insulated with a molded silicone skirted insulator. There is a four-skirt design rated 25/28 kV, and an eight-skirt design rated 35 kV. Cold Shrink QT-II terminations are provided in an expanded state, mounted on a removable inner supporting plastic core. As supplied in this prestretched condition the termination is ready for field installation. During installation the core is unwound, allowing the termination to shrink and form a tight seal. Collectively, these terminations kits accommodate cable primary insulation diameters from .632” to 2.75” (16-70 mm). These kits can be used to terminate the following concentric neutral (CN) power cables: #2 AWG to 1250 kcmil at 15 kV; #2 AWG to 1500 kcmil at 25 kV and #2 AWG to 2000 kcmil at 35 kV.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 1200 psiSilicone Rubber Insulator; ASTM D42-68
 1394 psiEPDM Rubber Hi-K Stress Control Tube; ASTM D42-68
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.7
@Temperature 130 °C
Silicone Rubber Insulator; ASTM D150-70
 3.0
@Temperature 90.0 °C
Silicone Rubber Insulator; ASTM D150-70
 3.4
@Temperature 23.0 °C
Silicone Rubber Insulator; ASTM D150-70
 20
@Frequency 100000 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150-70
 24
@Frequency 10000 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150-70
 29
@Frequency 1000 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150-70
 35
@Frequency 150 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150-70
 24.5
@Frequency 60.0 Hz,
Temperature 65.0 °C
EPDM Rubber Hi-K Stress Control Tube, 400 V at 60% Strain; ASTM D150-70
 25.2
@Frequency 60.0 Hz,
Temperature 90.0 °C
EPDM Rubber Hi-K Stress Control Tube, 400 V at 60% Strain; ASTM D150-70
 25.7
@Frequency 60.0 Hz,
Temperature 23.0 °C
EPDM Rubber Hi-K Stress Control Tube, 400 V at 60% Strain; ASTM D150-70
 27.2
@Frequency 60.0 Hz,
Temperature 65.0 °C
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150-70
 27.7
@Frequency 60.0 Hz,
Temperature 90.0 °C
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150-70
 28.8
@Frequency 60.0 Hz,
Temperature 23.0 °C
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150-70
Dielectric Strength 507 kV/in
@Thickness 0.190 mm
Silicone Rubber Insulator; ASTM D149-70
Dissipation Factor 0.12
@Frequency 100000 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150-70
 0.14
@Frequency 10000 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150-70
 0.15
@Frequency 1000 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150-70
 0.16
@Frequency 150 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150-70
 0.093
@Frequency 60.0 Hz,
Temperature 65.0 °C
EPDM Rubber Hi-K Stress Control Tube, 400 V at 60% Strain; ASTM D150-70
 0.096
@Frequency 60.0 Hz,
Temperature 23.0 °C
EPDM Rubber Hi-K Stress Control Tube, 400 V at 60% Strain; ASTM D150-70
 0.132
@Frequency 60.0 Hz,
Temperature 90.0 °C
EPDM Rubber Hi-K Stress Control Tube, 400 V at 60% Strain; ASTM D150-70
 0.161
@Frequency 60.0 Hz,
Temperature 90.0 °C
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150-70
 0.165
@Frequency 60.0 Hz,
Temperature 65.0 °C
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150-70
 0.166
@Frequency 60.0 Hz,
Temperature 23.0 °C
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150-70
Track Resistance 36000 sec2.5 kV, 10 k Ohms; ASTM 2303-68

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Silicone Rubber
Momentive Performance Materials Silplus™ 60 CW Heat Cured Rubber - Cable & Wire
Momentive Performance Materials Silopren™ Electro 242-0 Electrically Insulating Liquid Silicone Rubber
3M RJS--1 3/C Phase Rejacketing System
3M 8560 Cold Shrink Silicone Rubber 3/C Cable Breakout Boots

PMM35162 / 169909

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.