MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Unifrax Fiberfrax® Fiberwall® 304 SS Systems Hardware
Categories: Ceramic

Material Notes: The Fiberwall® systems family of anchoring hardware and accessory components provides an array of attachment options to cover a broad range of lining system designs and application requirements. Intended for use with Fiberfrax Fiberwall lining systems, Fiberwall hardware is available in a variety of metal alloy grades as well as in various ceramic compositions. This family of hardware components has been developed to provide optimal service life for an assortment of Fiberwall lining systems including layered blanket and board linings, stackbond linings, Hefty-Loc™ bonded modular systems and L.O.R. (lining over refractory) linings.

Information Provided by Unifrax I LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield  0.124 MPa
@Temperature 1000 °C
18.0 psi
@Temperature 1830 °F
 0.262 MPa
@Temperature 25.0 °C
38.0 psi
@Temperature 77.0 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 760 °C1400 °FRecommended Operating Temperature
 
Descriptive Properties
Chemical CompositionHigh alumina (Al2O3)
Temperature Grade (°C)1510Max

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type 304L Stainless Steel
304 Stainless Steel (UNS S30400); Hot Finished and Annealed Bar and Forgings
304 Stainless Steel (UNS S30400); Annealed Wire
304 Stainless Steel (UNS S30400); Cold Finished and Annealed Bar
AISI Type 304HN Stainless Steel

CUNIF091 / 97863

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.