MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Dow Dow™ DMDA-8933 NT 7 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Product Description: Dow DMDA-8933 NT 7 HDPE is produced via UNIPOL™ Process Technology from Dow and is intended for use in a broad range of injection molding applications such as injection molded containers and thin-walled pails. The product is specifically designed to provide excellent processing in all injection molding equipment.
  • Injection molding
  • Narrow molecular weight distribution
  • Excellent balance of toughness, and stress crack resistance
Complies with: US FDA 21 CFR 177.1520©3.2a; Canadian HPFB No Objection. Consult the regulations for complete details.

Availability: Asia Pacific; Latin America; North America

Agency Ratings: FDA 21 CFR 177.1520©3.2a; Canadian HPFB No Objection

Form: Pellets

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³ASTM D792
Melt Flow 33 g/10 min
@Load 2.16 kg,
Temperature 190 °C
33 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 13.8 MPa2000 psiPlaque molded and tested in accordance with ASTM D4976; ASTM D638
Tensile Strength, Yield 26.9 MPa3900 psiPlaque molded and tested in accordance with ASTM D4976; ASTM D638
Flexural Modulus 1.00 GPa145 ksi2% Secant, Procedure B, Plaque molded and tested in accordance with ASTM D4976; ASTM D790B
 
Thermal PropertiesMetricEnglishComments
Melting Point 126 °C259 °FPlaque molded and tested in accordance with ASTM D4976
Crystallization Temperature 108 °C226 °FPlaque molded and tested in accordance with ASTM D4976

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDOWF451 / 311144

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.