MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow LDPE 641I Low Density Polyethylene, Liner Film Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: DOW LDPE 641I resin is a general purpose liner film resin for thin gauge applications requiring good drawdown and excellent toughness. It contains medium levels of slip additive and low levels of antiblock additive. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for food contact applications. The regulation should be consulted for complete details.

Film properties below based on a film thickness of 40 µm. Data provided by Dow Chemical.

Key Words: Dow PE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.922 g/cc
Thickness 40.0 microns
Melt Flow 2.0 g/10 min
@Load 2.16 kg
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 11.4 MPa
Film Tensile Strength at Yield, TD 10.3 MPa
Film Elongation at Break, MD 290 %
Film Elongation at Break, TD 560 %
Coefficient of Friction 0.10
Elmendorf Tear Strength MD 520 g
Elmendorf Tear Strength TD 250 g
Elmendorf Tear Strength, MD 13.0 g/micron
Elmendorf Tear Strength, TD 6.30 g/micron
Dart Drop 2.40 g/micron
Film Tensile Strength at Break, MD 25.9 MPa
Film Tensile Strength at Break, TD 17.6 MPa
 
Optical PropertiesOriginal ValueComments
Haze 8.5 %
Gloss 61 %45°
 
Processing PropertiesOriginal ValueComments
Processing Temperature 191 °CFilm extrusion temperature
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow LDPE 640I Low Density Polyethylene, Liner Film Grade
Dow LDPE 955I Low Density Polyethylene
Dow LDPE 133A Low Density Polyethylene, Blown Film Grade
Dow LDPE 135A Low Density Polyethylene, Blown Film Grade
Dow LDPE 5004IM Low Density Polyethylene

PDW509 / 34578

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.