MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Arkema Kynar® Film 502 CUH HC PVDF
Categories: Polymer; Film

Material Notes:

Information provided by Arkema.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 29.0 MPa4210 psiDry; ISO 527-3
Film Tensile Strength at Yield, TD 29.0 MPa4210 psiDry; ISO 527-3
Film Elongation at Break, MD 50 %50 %Dry; ISO 527-3
Film Elongation at Break, TD 50 %50 %Dry; ISO 527-3
Film Elongation at Yield, MD 3.5 %3.5 %Dry; ISO 527-3
Film Elongation at Yield, TD 3.5 %3.5 %Dry; ISO 527-3
Tear Strength 2.00 kN/m11.4 pliTrouser Tear Resistance, parallel dry; ISO 6383-1
 3.00 kN/m17.1 pliTrouser Tear Resistance, normal dry; ISO 6383-1
Film Tensile Strength at Break, MD 30.0 MPa4350 psiDry; ISO 527-3
Film Tensile Strength at Break, TD 25.0 MPa3630 psiDry; ISO 527-3
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 100 kV/mm2540 kV/inDry; IEC 60243-1
 
Descriptive Properties
Light StabilizedYes
Moisture SensitiveNo

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema Kynar® Film 252 PGM TR PVDF
Mitsubishi Hostaphan® RN, 350 micron Nominal Thickness Universal Polyethylene Terephthalate Film
Covestro Makrofol® DE 6-2 Polycarbonate
Braskem HP 523J Bioriented Film Polypropylene
Armacell ArmaFORM® PET Foil 300

PARKF749 / 193541

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.