MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow 4012 Low Density Polyethylene (LDPE)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Polyethylene 4012 is used for a variety of applications such as condiment packaging, dry and moist foods packaging, sugar pouches, lidding stock and medical packaging.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.918 g/ccASTM D792
Water Vapor Transmission 27.9 g/m²/dayat 1 atm; 1.0 mil coating onto 50 lb Kraft paper; ASTM F1249
Thickness >= 0.300 milCoating Thickness; Extrusion Coating Processability; Dow Method
Melt Index of Compound 12 g/10 minASTM D1238
Neck In 4.80 cm610°F and 1.0 mil; Extrusion Coating Processability; Dow Method
Coating Weight >= 4.00 lb/reamExtrusion Coating Processability; Dow Method
 
Mechanical PropertiesOriginal ValueComments
Coefficient of Friction, Dynamic 0.60(film/film); 1.0 mil coating onto 50 lb Kraft paper; ASTM D1894
Heat Seal Strength Initiation Temperature 105 °C1 lb/in heat seal strength; 1.0 mil coating onto 50 lb Kraft paper; Dow Method
 
Thermal PropertiesOriginal ValueComments
Melting Point 107 °CDow Method (DSC)
Vicat Softening Point 89.0 °CASTM D1525
 
Processing PropertiesOriginal ValueComments
Melt Temperature 315 - 327 °CExtrusion Coating Processability
 
Descriptive Properties
Line Speed fpm, max1610Dow Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont 20 Series 20-6064 Specialty Polyethylene Resin
Dow 4010 Low Density Polyethylene (LDPE)
Dow 611A Low Density Polyethylene (LDPE)
Dow 620I Linear Low Density Polyethylene (LDPE)
Dow 662I Low Density Polyethylene Resin

PDOW1225 / 30443

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.