MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Kolon CY412 Silicone Release Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: Good Chemical Resistance (MEK, Toluene, Acetone). PET film coated with solvent-based silicone applied on outside. CY has good smear, rub-off , retained adhesion properties. Its good release property can be applicable to OCA Protection uses.

Information provided by Kolon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Coefficient of Friction, Dynamic  0.090
@Thickness 0.0250 mm
0.090
@Thickness 0.000984 in
ASTM D1894
 0.11
@Thickness 0.0380 mm
0.11
@Thickness 0.00150 in
ASTM D1894
Coefficient of Friction, Static  0.090
@Thickness 0.0250 mm
0.090
@Thickness 0.000984 in
ASTM D1894
 0.12
@Thickness 0.0380 mm
0.12
@Thickness 0.00150 in
ASTM D1894
Seal Strength 14.4 g/25 mm14.4 g/inRelease Force; FINAT-10
 14.6 g/25 mm14.6 g/inRelease Force; FINAT-10
 
Thermal PropertiesMetricEnglishComments
Shrinkage, MD  0.74 %
@Thickness 0.0380 mm
0.74 %
@Thickness 0.00150 in
Heat Shrinkage; ASTM D2305
 0.87 %
@Thickness 0.0250 mm
0.87 %
@Thickness 0.000984 in
Heat Shrinkage; ASTM D2305
Shrinkage, TD  0.00 %
@Thickness 0.0250 mm
0.00 %
@Thickness 0.000984 in
Heat Shrinkage; ASTM D2305
 0.00 %
@Thickness 0.0380 mm
0.00 %
@Thickness 0.00150 in
Heat Shrinkage; ASTM D2305
 
Optical PropertiesMetricEnglishComments
Haze  2.28 %
@Thickness 0.0250 mm
2.28 %
@Thickness 0.000984 in
ASTM D1003
 3.45 %
@Thickness 0.0380 mm
3.45 %
@Thickness 0.00150 in
ASTM D1003

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kolon CY312 Silicone Release Film
Solvay E2760 Release Film
Solvay P720X PET-Based Release Film
Chi Mei Acryrex® CM-211 PMMA
Kolon CY201 Silicone Release Film

PKOKZ813 / 185356

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.