Notes: MDF463 is a 15% glass fiver reinforced grade of nylon 6 that contains an impact modification system which offers superior low temperature performance – along with a stabilization package to enhance component life in severe environmental conditions. This grade offers a good balance of rigidity and toughness over a wide temperature range. Availability: Europe Fillers/Reinforcement: Glass Fiber, 15% Filler by Weight Additive: Heat Stabilizer; Impact Modifier Features: Heat Stabilized; Impact Modified; Low Temperature Impact Resistance; Low Temperature Toughness Processing Method: Injection Molding Information provided by Teknor Apex |