MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Copper, UNS C51100, HR04 Temper, Flat Products
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Hard and Stress Relieved

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Butt Weld, Capacity for Being Cold Worked; Good Suitability – Gas Shielded Arc Welding, Spot Weld; Fair Suitability – Oxyacetylene Welding, Coated Metal Arc Welding, Seam Weld; Poor Suitability – Capacity for Being Hot Formed

Common Fabrication Processes: Blanking; Drawing; Forming and Bending; Roll Threading and Knurling; Shearing; Stamping

Typical uses: Bridge Bearing Plates; Electrical Connectors; Fuse Clips; Switch Parts; Terminals; Fasteners; Lock Washers; Beater Bar; Bellows; Chemical hardware; Clutch Disks; Diaphragms; Perforated Sheets; Sleeve Bushings; Springs; Textile machinery

Applicable Specifications: Bar – ASTM B103/B103M; Bearings & Busings – MILITARY MIL-B-13501; Plate – ASTM B103/B103M; Bridge and Bearing ASTM B100; Sheet - Bridge and Bearing ASTM B100, ASTM B103/B103M; Strip – ASTM B103/B103M, ASTM B888/B88M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.320 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 80.0 ksi
Tensile Strength, Yield 73.0 ksi0.2% Offset
Elongation at Break 15 %
Tensile Modulus 16000 ksi
Modulus of Rigidity 6000 ksi
Poissons Ratio 0.33Calculated
Machinability 20 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000860 ohm-cm20% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.90 µin/in-°F
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.0900 BTU/lb-°F
Thermal Conductivity 48.4 BTU-in/hr-ft²-°F
Melting Point 1785 - 1945 °F
Solidus 1785 °F
Liquidus 1945 °F
Annealing Point 900 - 1250 °F
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 94.3 - 96.5 %As Balance
Iron, Fe <= 0.10 %
Lead, Pb <= 0.050 %
Phosphorus, P 0.030 - 0.35 %
Tin, Sn 3.5 - 4.9 %
Zinc, Zn <= 0.30 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC51100x2 / 292999

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.