System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
ExxonMobil Pax-Plus™ 3208 Blown Film Resin
(discontinued **)
Categories:
Polymer
;
Film
;
Thermoplastic
;
Polyethylene (PE)
;
High Density (HDPE)
;
High Density Polyethylene (HDPE), Film Grade
Material Notes:
Pax-Plus 3208 is a rubber modified high density polyethylene film resin offering good physical properties with ease of processing. It exhibits toughness, stress crack resistance and low WVTR.
Information provided by ExxonMobil Chemical
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
0.936
g/cc
ExxonMobil Method
Thickness
2.00
mil
Melt Flow
0.10
g/10 min
@Load 2.16 kg,
Temperature 190 °C
ExxonMobil Method
2.6
g/10 min
@Load 10.0 kg,
Temperature 190 °C
ExxonMobil Method
Mechanical Properties
Original Value
Comments
Film Tensile Strength at Yield, MD
1720
psi
at 2% offset; ASTM D882
Film Tensile Strength at Yield, TD
1900
psi
at 2% offset; ASTM D882
Film Elongation at Break, MD
630 %
ASTM D882
Film Elongation at Break, TD
750 %
ASTM D882
Puncture Energy
1.575
ft-lb
Exxon Mobil Method
Elmendorf Tear Strength MD
70
g
ASTM D1922
Elmendorf Tear Strength TD
570
g
ASTM D1922
Elmendorf Tear Strength, MD
35.0
g/mil
ASTM D1922
Elmendorf Tear Strength, TD
285
g/mil
ASTM D1922
Dart Drop
125
g/mil
ASTM D1709
Dart Drop Test
250
g
ASTM D1709
Film Tensile Strength at Break, MD
3730
psi
ASTM D882
Film Tensile Strength at Break, TD
3420
psi
ASTM D882
1% Secant Modulus, MD
47100
psi
ASTM D882
1% Secant Modulus, TD
58900
psi
ASTM D882
Thermal Properties
Original Value
Comments
Melting Point
263
°F
Peak Melting Temperature; ExxonMobil Method
Vicat Softening Point
234
°F
ExxonMobil Method
Descriptive Properties
Features
Thermal Stabilizer
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Dow DOWLEX™ 2071 Linear Low Density Polyethylene
ExxonMobil HD 7960.13 HMW Blown Film Resin
Dow LDPE 682I Low Density Polyethylene, Film Grade
Dow LDPE 527A Low Density Polyethylene, Blown Film Grade
Dow LDPE 493A Low Density Polyethylene, Film Grade
PEXB114 / 37419
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.