MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Sumitomo Bakelite E 2748A Epoxy Molding Compound
Categories: Polymer; Thermoset; Epoxy; Epoxy Molding Compound

Material Notes: E 2748A is a glass reinforced epoxy molding compound, with good impact strength combined with soft flow for the encapsulation of devices requiring high quality and thermal shock resistance.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.76 g/cc1.76 g/ccASTM D792
Apparent Bulk Density 0.700 g/cc0.0253 lb/in³Powder; ASTM D1895
Water Absorption 0.20 %
@Time 173000 sec
0.20 %
@Time 48.0 hour
ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 76.0 MPa11000 psiASTM D638
Flexural Strength 142 MPa20600 psiASTM D790
Flexural Modulus 12.4 GPa1800 ksiASTM D790
Compressive Strength 210 MPa30500 psiASTM D695
Izod Impact, Notched 0.310 J/cm0.581 ft-lb/inASTM D256A
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 4.5
@Frequency 1e+6 Hz
4.5
@Frequency 1e+6 Hz
wet; ASTM D150
Dielectric Strength >= 14.2 kV/mm
@Frequency 60 Hz
>= 361 kV/in
@Frequency 60 Hz
ST, dry
Dissipation Factor 0.010
@Frequency 1e+6 Hz
0.010
@Frequency 1e+6 Hz
wet; ASTM D150
Arc Resistance 180 sec180 secASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 17.0 µm/m-°C9.44 µin/in-°FASTM E831

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elektro-Isola G-Etronax EP FR4 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets
Cosmic Plastics E4940P Mineral/Glass Filled Epoxy Molding Compound
Sumitomo Bakelite E 7459A Epoxy Molding Compound
Sumitomo Bakelite E 3938A Epoxy Molding Compound
Sumitomo Bakelite E 3812 M-1 Epoxy Molding Compound

PSUMIT128 / 193933

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.