Product Description: A metalized biaxially oriented polypropylene film, metalized on one side, heat sealable on the other side. It is typically used in lamination with other substrates on HFFS and VFFS applications. Availability: Africa & Middle East, Asia Pacific and Europe Key Features: - Excellent adhesion of aluminum to film
- Excellent moisture barrier
- Excellent light barrier
- Good hot tack
- High yield
- Easy to convert
- Brilliant metal appearance
Features:- In Lamination Lap Sealable
- Light Barrier
- Moisture Barrier
Applications:- Bakery
- Biscuits/Cookie/Crackers
- Box Overwrap
- Confectionery, Chocolate
- Confectionery, Gum
- Confectionery, Sugar
- Crisps and Snacks
- Frozen Food
- Ice Cream
- Pet Food
Uses: - HFFS Flexible Packaging
- Pre-made Bags – Flexible Packaging
- VFFS Flexible Packaging
Processing Method: Cold Seal Adhesive, Inner Web Adhesive Lamination, Solvent Flexographic Printing, Solvent Rotogravure Printing and Surface Print UnsupportedInformation provided by ExxonMobil |