MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Teknor Apex Laripur® LPR 9060HFM Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Features:

- Excellent performance under extreme and aggressive environments - Superior abrasion and cut resistance - Resistance to chemical, microbial attack and hydrolysis - Excellent flexibility at low temperatures - Good weathering properties - Non-halogen flame retardant

- Low Gloss

Applications:

- Energy & Power Cables: coiled or spiral: Construction / Mining - Automotive Cables: Anti-lock Braking Systems – ABS - Industrial Cables: Traffic / Signal / Trains / Boats / Buildings - Geophysical Cables: Land & Off-shore; Marine, Sub-sea & Umbilical - Telecommunications Cables: Telephone & Data Transmission; Military and Fiber Optics - Audio and Medical Cables

Information Provided by Teknor Apex

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.22 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 89ASTM D2240
Tensile Strength 4930 psiASTM D412
Tensile Stress at Strain 1075 psi
@Strain 50 %
ASTM D412
 1405 psi
@Strain 100 %
ASTM D412
 1885 psi
@Strain 300 %
ASTM D412
Elongation at Break 615 %ASTM D412
Tear Strength 348 kN/mASTM D624
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 183 °FASTM D1525
Flammability, UL94 V-0
@Thickness 1.00 mm
 V-0
@Thickness 2.00 mm
 V-0
@Thickness 6.00 mm
 
Descriptive Properties
Abrasion Loss (mm3)50DIN 53516

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teknor Apex Laripur® LPR 9060EM Thermoplastic Polyurethane
RTP Company RTP 1299 X 101066 Ether-based Thermoplastic Polyurethane Elastomer, Glass Bubbles
Teknor Apex Laripur® LPR 7560EG Thermoplastic Polyurethane
Teknor Apex Tekbond® TB 1139A Thermoplastic Elastomer
Teknor Apex Medalist® MD-230 Thermoplastic Elastomer

PTEKNO868 / 129049

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.