MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Osterman & Co Osterlene® LLO1020SA LLDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: Product Description: LLO1020 is designed for production of a wide variety of films. Films made from this resin exhibit a combination of good toughness and tear resistance.

Availability: North America
Additive: Antiblock: 3000 ppm; Slip: 1200 ppm
Features: Good Tear Strength; Good Toughness
Uses: Film; Food Packaging

Information provided by Osterman & Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³ASTM D792
Melt Flow 0.95 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.95 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Antiblock Level 3000 ppm3000 ppm
Slip Level 1200 ppm1200 ppm
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 12.5 MPa1820 psiASTM D882
Film Tensile Strength at Yield, TD 13.4 MPa1950 psiASTM D882
Film Elongation at Break, MD 730 %730 %ASTM D882
Film Elongation at Break, TD 810 %810 %ASTM D882
Secant Modulus, MD 0.181 GPa26.3 ksiASTM D790
Secant Modulus, TD 0.166 GPa24.1 ksiASTM D790
Elmendorf Tear Strength MD 810 g810 gASTM D1922
Elmendorf Tear Strength TD 1100 g1100 gASTM D1922
Dart Drop Test 300 g0.662 lbASTM D1709
Film Tensile Strength at Break, MD 52.0 MPa7540 psiASTM D882
Film Tensile Strength at Break, TD 44.5 MPa6450 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 121 °C250 °F
Vicat Softening Point 108 °C226 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 11 %11 %ASTM D1003
Gloss 30 %30 %45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

POSTER131 / 267713

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.